Thermophysical Properties of Liquids and Solidification Microstructure Characteristics—Benchmark Data Generated in Microgravity

By
Hans J. Fecht
Hans J. Fecht
Ulm University
,
Germany
Search for other works by this author on:
Bernard Billia
Bernard Billia
Aix-Marseille Université and CNRS
,
France
Search for other works by this author on:
Published:
2010
Page range:
8 - 17
Publication history
June 30, 2010

Abstract

For a wide range of new or better products, solidification processing of metallic materials from the melt is a step of uppermost importance in the industrial production chain. This article discusses the casting and solidification of molten metallic alloy along with the application of low-gravity platforms and facilities for solidification processing. It provides a description of dendritic growth studies and electromagnetic levitation. The article concludes with information on the in situ and real-time monitoring of solidification processing.

You do not currently have access to this content.
Don't already have an account? Register

Hans J. Fecht, Bernard Billia, 2010. "Thermophysical Properties of Liquids and Solidification Microstructure Characteristics—Benchmark Data Generated in Microgravity", Metals Process Simulation, D.U. Furrer, S.L. Semiatin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal