Skip to Main Content
ASM Handbook

Metals Process Simulation

Edited by
D.U. Furrer
D.U. Furrer
Search for other works by this author on:
S.L. Semiatin
S.L. Semiatin
Search for other works by this author on:
ASM International
Volume
22B
ISBN electronic:
978-1-62708-197-9
Publication date:
2010
Book Chapter

Design Optimization Methodologies

By
Alex Van der Velden
Alex Van der Velden
SIMULIA
Search for other works by this author on:
Patrick Koch
Patrick Koch
SIMULIA
Search for other works by this author on:
Santosh Tiwari
Santosh Tiwari
SIMULIA
Search for other works by this author on:
Published:
2010
Page range:
614 - 624
Publication history
March 19, 2010

Abstract

The process of optimization involves choosing the best solution from a pool of potential candidate solutions. This article provides a description of some classes of problems and the optimization methods that solve them. These problems include the deterministic single-objective problem, the deterministic multiobjective problem, and the nondeterministic, stochastic optimization problem. The article presents several complementary approaches to solve a wide variety of single-objective and multiobjective mechanical engineering applications. Multiobjective optimization study and stochastic optimization studies are also discussed.

You do not currently have access to this content.
Don't already have an account? Register

Alex Van der Velden, Patrick Koch, Santosh Tiwari, 2010. "Design Optimization Methodologies", Metals Process Simulation, D.U. Furrer, S.L. Semiatin