Skip to Main Content
ASM Handbook

Metals Process Simulation

Edited by
D.U. Furrer
D.U. Furrer
Search for other works by this author on:
S.L. Semiatin
S.L. Semiatin
Search for other works by this author on:
ASM International
Volume
22B
ISBN electronic:
978-1-62708-197-9
Publication date:
2010
Book Chapter

Modeling of Hot Isostatic Pressing

By
Victor Samarov
Victor Samarov
Synertech P/M Inc.
Search for other works by this author on:
Vassily Goloveshkin
Vassily Goloveshkin
LNT
Search for other works by this author on:
Published:
2010
Page range:
335 - 342
Publication history
March 05, 2010

Abstract

This article discusses the two major applications of hot isostatic pressing (HIP), such as healing of inherent internal defects in castings and welds, and consolidation of powder materials. It describes the design principles of the HIP tooling, as well as the problems associated with mathematical modeling of HIP. The article presents an example for the modeling process of the HIP. It reviews the numerical modeling and tooling design of a casing component demonstration.

You do not currently have access to this content.
Don't already have an account? Register

Victor Samarov, Vassily Goloveshkin, 2010. "Modeling of Hot Isostatic Pressing", Metals Process Simulation, D.U. Furrer, S.L. Semiatin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal