Modeling of Microstructure Evolution during the Thermomechanical Processing of Nickel-Base Superalloys

By
J.P. Thomas
J.P. Thomas
ATI Allvac, an Allegheny Technologies company
Search for other works by this author on:
F. Montheillet
F. Montheillet
CNRS, Ecole Nationale Supérieure des Mines de Saint-Etienne
Search for other works by this author on:
S. L. Semiatin
S. L. Semiatin
Air Force Research Laboratory
Search for other works by this author on:
Published:
2009
Page range:
566 - 582
Publication history
August 19, 2009

Abstract

This article summarizes the general features of microstructure evolution during the thermomechanical processing (TMP) of nickel-base superalloys and the challenges posed by the modeling of such phenomena. It describes the fundamentals and implementations of various modeling methodologies. These include JMAK (Avrami) models, topological models, and mesoscale physics-based models.

You do not currently have access to this content.
Don't already have an account? Register

J.P. Thomas, F. Montheillet, S. L. Semiatin, 2009. "Modeling of Microstructure Evolution during the Thermomechanical Processing of Nickel-Base Superalloys", Fundamentals of Modeling for Metals Processing, D.U. Furrer, S.L. Semiatin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal