Skip to Main Content
ASM Handbook

Fundamentals of Modeling for Metals Processing

Edited by
D.U. Furrer
D.U. Furrer
Search for other works by this author on:
S.L. Semiatin
S.L. Semiatin
Search for other works by this author on:
ASM International
Volume
22A
ISBN electronic:
978-1-62708-196-2
Publication date:
2009
Book Chapter

Modeling Diffusion in Binary and Multicomponent Alloys

By
John Morral
John Morral
The Ohio State University
Search for other works by this author on:
Frederick Meisenkothen
Frederick Meisenkothen
UES, Inc./Air Force Research Laboratory
Search for other works by this author on:
Published:
2009
Page range:
155 - 170
Publication history
July 25, 2009

Abstract

This article presents various equations that are essential for the modeling of both single-phase and multiphase profiles. It includes the fundamental laws of diffusion, along with its equations and solutions. The article provides information on the series of applications that illustrate how various diffusional processes can be modeled.

You do not currently have access to this content.
Don't already have an account? Register

John Morral, Frederick Meisenkothen, 2009. "Modeling Diffusion in Binary and Multicomponent Alloys", Fundamentals of Modeling for Metals Processing, D.U. Furrer, S.L. Semiatin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal