Skip to Main Content
ASM Handbook

Fundamentals of Modeling for Metals Processing

Edited by
D.U. Furrer
D.U. Furrer
Search for other works by this author on:
S.L. Semiatin
S.L. Semiatin
Search for other works by this author on:
ASM International
Volume
22A
ISBN electronic:
978-1-62708-196-2
Publication date:
2009
Book Chapter

Modeling of Microstructure Evolution during the Thermomechanical Processing of Titanium Alloys

By
S.L. Semiatin
S.L. Semiatin
Air Force Research Laboratory
Search for other works by this author on:
D.U. Furrer
D.U. Furrer
Rolls-Royce Corporation
Search for other works by this author on:
Published:
2009
Page range:
522 - 535
Publication history
July 13, 2009

Abstract

This article focuses on the modeling of microstructure evolution during thermomechanical processing in the two-phase field for alpha/beta and beta titanium alloys. It also discusses the mechanisms of spheroidization, the coarsening, particle growth, and phase decomposition in titanium alloys, with their corresponding equations.

You do not currently have access to this content.
Don't already have an account? Register

S.L. Semiatin, D.U. Furrer, 2009. "Modeling of Microstructure Evolution during the Thermomechanical Processing of Titanium Alloys", Fundamentals of Modeling for Metals Processing, D.U. Furrer, S.L. Semiatin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal