Skip to Main Content
ASM Handbook

Fundamentals of Modeling for Metals Processing

Edited by
D.U. Furrer
D.U. Furrer
Search for other works by this author on:
S.L. Semiatin
S.L. Semiatin
Search for other works by this author on:
ASM International
Volume
22A
ISBN electronic:
978-1-62708-196-2
Publication date:
2009
Book Chapter

Phase Equilibria and Phase Diagram Modeling

By
Y.A. Chang
Y.A. Chang
University of Wisconsin
Search for other works by this author on:
H.-B. Cao
H.-B. Cao
University of Wisconsin
Search for other works by this author on:
S.-L. Chen
S.-L. Chen
CompuTherm, LLC
Search for other works by this author on:
F. Zhang
F. Zhang
CompuTherm, LLC
Search for other works by this author on:
Y. Yang
Y. Yang
CompuTherm, LLC
Search for other works by this author on:
W. Cao
W. Cao
CompuTherm, LLC
Search for other works by this author on:
K. Wu
K. Wu
CompuTherm, LLC
Search for other works by this author on:
Published:
2009
Page range:
443 - 457
Publication history
July 25, 2009

Abstract

A phase diagram is a graphical representation of the phase equilibria of materials in terms of temperature, composition, and pressure. This article provides an overview on the background of phase diagram calculation software. It presents an algorithm to calculate binary stable phase equilibria. The article summarizes a rapid method to obtain a thermodynamic description of a multicomponent system. It also provides information on thermodynamically calculated phase diagrams.

You do not currently have access to this content.
Don't already have an account? Register

Y.A. Chang, H.-B. Cao, S.-L. Chen, F. Zhang, Y. Yang, W. Cao, K. Wu, 2009. "Phase Equilibria and Phase Diagram Modeling", Fundamentals of Modeling for Metals Processing, D.U. Furrer, S.L. Semiatin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal