Determination of Heat Transfer Coefficients for Thermal Modeling

By
D. Scott MacKenzie
D. Scott MacKenzie
Houghton International, Inc.
Search for other works by this author on:
Andrew L. Banka
Andrew L. Banka
Airflow Sciences Corporation
Search for other works by this author on:
Published:
2009
Page range:
106 - 126
Publication history
August 31, 2009

Abstract

This article provides information on the various stages of quenching, sources of distortion, and factors that affect the creation of thermal gradients. It reviews the various determinations of heat-transfer coefficients by the thermal conductivity and diffusivity method, analytical and empirical methods, application of cooling curves, computational fluid dynamics, and the inverse conduction calculation and measurement of parts. Suitable examples are also provided.

You do not currently have access to this content.
Don't already have an account? Register

D. Scott MacKenzie, Andrew L. Banka, 2009. "Determination of Heat Transfer Coefficients for Thermal Modeling", Fundamentals of Modeling for Metals Processing, D.U. Furrer, S.L. Semiatin