Crystal-Plasticity Fundamentals

By
Henry R. Piehler
Henry R. Piehler
Carnegie Mellon University
Search for other works by this author on:
Published:
2009
Page range:
232 - 238
Publication history
April 13, 2009

Abstract

This article presents the Schmid's law that describes the response of crystal structures to loading. It describes the Taylor model to calculate the uniaxial yield stress of an isotropic face-centered cubic aggregate in terms of critical resolved shear stress. The article discusses the stress-based approach of the Bishop and Hill procedure to directly find stress states that could simultaneously operate at least five independent slip systems. It presents ways to find isostress or lower-bound yield loci for sheets having single-crystal orientation.

You do not currently have access to this content.
Don't already have an account? Register

Henry R. Piehler, 2009. "Crystal-Plasticity Fundamentals", Fundamentals of Modeling for Metals Processing, D.U. Furrer, S.L. Semiatin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal