This article is a comprehensive collection of the thermodynamic equations and property relations of the first and second laws of thermodynamics that are applicable to closed-system consisting of several homogeneous and heterogeneous phases.

Abstract

This article is a comprehensive collection of formulas, tables, and analytical solutions, addressing hundreds of heat-transfer scenarios encountered in science and engineering. It also demonstrates how to set up and solve real-world problems, while accounting for material properties, environmental variables, boundary and state conditions, and the primary modes of heat transfer: conduction, convection, and radiation.

Abstract

This article is a comprehensive collection of fluid dynamic equations for properties of fluids, fluid statics, fluid motion, dimensional analysis, and boundary layer flow. It presents equations for analyzing problems in fluid mechanics, continuity equation, momentum equation, and energy equation for solving various problems related to fluid dynamics.

You do not currently have access to this content.
Don't already have an account? Register

2009. "Reference Information", Fundamentals of Modeling for Metals Processing, D.U. Furrer, S.L. Semiatin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal