Abstract

This article presents a diagramatic representation of a periodic system that illustrates the fundamental alloying nature of iron for ferrous metallurgists.

Abstract

This article presents a comprehensive collection of tables that list fundamental physical constants, standard atomic weights, melting points, atomic size parameters, heats of transition, thermal properties, temperature-dependent allotropic structures, pressure-dependent allotropic structures, and magnetic phase transition temperatures of the elements.

Abstract

This article contains a table that lists the density of metals and alloys. It presents information on aluminum, copper, iron, lead, magnesium, nickel, tin, titanium, and zinc, an their respective alloys. Information on wrought alloys, permanent magnet materials, precious metals, and rare earth metals is also listed.

You do not currently have access to this content.
Don't already have an account? Register

2009. "Physical Data on the Elements and Alloys", Fundamentals of Modeling for Metals Processing, D.U. Furrer, S.L. Semiatin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal