Material and Chemical Characterization as a Part of the Biological Evaluation of Medical Devices

By
David E. Albert
David E. Albert
NAMSA
Search for other works by this author on:
Published:
2012
Page range:
323 - 330
Publication history
June 19, 2012

Abstract

This article provides the background of biological evaluation of medical devices. It discusses what the ISO 10993 standards require for polymeric biomaterials and presents examples of what qualitative and quantitative tests can be used to satisfy the requirements. The article describes infrared (IR) analysis and thermal analyses that are used extensively to fingerprint polymeric materials and should be a part of all polymeric biomaterials characterization programs. It also provides a discussion on the chemical characterization and risk assessment of extracts. Background information on risk assessments of extracts is also included. The four basic steps that are commonly used in the risk assessment process are discussed. These steps include hazard identification, dose-response assessment, and exposure assessment, and risk characterization.

You do not currently have access to this content.
Don't already have an account? Register

David E. Albert, 2012. "Material and Chemical Characterization as a Part of the Biological Evaluation of Medical Devices", Materials for Medical Devices, Roger J. Narayan

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal