Skip to Main Content
ASM Handbook

Materials for Medical Devices

Edited by
Roger J. Narayan
Roger J. Narayan
Search for other works by this author on:
ASM International
Volume
23
ISBN electronic:
978-1-62708-198-6
Publication date:
2012
Book Chapter

Surface Characterization for Medical Devices

By
Larry D. Hanke
Larry D. Hanke
Materials Evaluation and Engineering Inc.
Search for other works by this author on:
Published:
2012
Page range:
331 - 342
Publication history
June 19, 2012

Abstract

This article focuses on the modes of operation, physical basis, sample requirements, properties characterized, advantages, and limitations of common characterization methods that are used to evaluate the physical morphology and chemical properties of component surfaces for medical devices. The methods include light microscopy, scanning electron microscopy, atomic force microscopy, energy-dispersive x-ray spectroscopy, Auger electron spectroscopy, secondary ion mass spectrometry, x-ray photoelectron spectroscopy, Fourier transform infrared spectroscopy, and Raman spectroscopy.

You do not currently have access to this content.
Don't already have an account? Register

Larry D. Hanke, 2012. "Surface Characterization for Medical Devices", Materials for Medical Devices, Roger J. Narayan

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal