Shape Memory Alloys

By
Tom Duerig
Tom Duerig
Search for other works by this author on:
Published:
2012
Page range:
237 - 250
Publication history
June 25, 2012

Abstract

This article focuses on the specific aspects of nitinol that are of interest to medical device designers. It describes the physical metallurgy, physical properties, and tensile properties of the nitinol. The article discusses the factors influencing superelastic shape memory effects, fatigue, and corrosion in medical device design. It reviews the biocompatibility of nitinol based on corrosion behavior. The article describes the general principles, potential pitfalls, and key properties for manufacturing, heat treatment, and processing of nitinol.

You do not currently have access to this content.
Don't already have an account? Register

Tom Duerig, 2012. "Shape Memory Alloys", Materials for Medical Devices, Roger J. Narayan

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal