Tantalum

By
Sam Nasser
Sam Nasser
Wayne State University
Search for other works by this author on:
Published:
2012
Page range:
278 - 280
Publication history
June 25, 2012

Abstract

Physically, tantalum is a dark, blue-gray, lusterless metal that exists in two crystalline forms: an alpha-phase with a body-centered cubic structure, and a brittle beta-phase with a tetragonal orientation. This article tabulates the physical and material properties of tantalum. It discusses the use of tantalum in medical electronics and the advantage of tantalum over stainless steel. The article describes the manufacturing and medical applications of tantalum foam.

You do not currently have access to this content.
Don't already have an account? Register

Sam Nasser, 2012. "Tantalum", Materials for Medical Devices, Roger J. Narayan

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal