Skip to Main Content
ASM Handbook

Nondestructive Evaluation of Materials

Edited by
Aquil Ahmad
Aquil Ahmad
Search for other works by this author on:
Leonard J. Bond
Leonard J. Bond
Search for other works by this author on:
ASM International
Volume
17
ISBN electronic:
978-1-62708-190-0
Publication date:
2018
Book Chapter

Nondestructive Inspection of Tubular Products[1]

By
Lesley D. Frame
Lesley D. Frame
Revising author
University of Bridgeport
Search for other works by this author on:
Published:
2018
Page range:
566 - 589
Publication history
August 21, 2018

Abstract

This article provides information on the application of nondestructive examination (NDE) technologies to tube and pipe products. These include modeling and simulation methods, eddy-current methods, magnetic methods, acoustic methods, and physical methods. A summary of nondestructive examination methods based on flaw type and product stage is presented in a table. The article also discusses in-service inspection of tubular products and presents an example that illustrates the importance of nondestructive testing (NDT) for welds in austenitic stainless steel tubing.

You do not currently have access to this content.
Don't already have an account? Register

Lesley D. Frame, 2018. "Nondestructive Inspection of Tubular Products", Nondestructive Evaluation of Materials, Aquil Ahmad, Leonard J. Bond

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal