Nondestructive Testing of Composites (Polymer- and Metal-Matrix Composites)[1]

Published:
2018
Page range:
631 - 658
Publication history
August 21, 2018

Abstract

This article introduces the principal methodologies and some advanced technologies that are being applied for nondestructive evaluation (NDE) of fiber-reinforced polymer-matrix composites. These include acoustic emission, ultrasonic, eddy-current, computed tomography, electromagnetic acoustic transducer, radiography, thermography, and low-frequency vibration methods. The article also provides information on NDE methods commonly used for metal-matrix composites.

You do not currently have access to this content.
Don't already have an account? Register

2018. "Nondestructive Testing of Composites (Polymer- and Metal-Matrix Composites)", Nondestructive Evaluation of Materials, Aquil Ahmad, Leonard J. Bond

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal