Thermoelastic Stress Analysis

By
David Backman
David Backman
National Research Council Canada
Search for other works by this author on:
Published:
2018
Page range:
143 - 151
Publication history
August 21, 2018

Abstract

Thermoelastic stress analysis (TSA) an increasingly popular infrared (IR)-based technique for measuring stress on the surface of a part subjected to time-varying loads. This article begins by providing a theoretical and historical background of thermoelastic stress analysis. It then describes infrared detectors, such as quantum detectors and thermal/nonquantum detectors, for thermoelastic stress analysis. The article discusses the theoretical aspects for producing thermoelastic stress analysis data and the applications amenable to thermoelastic stress analysis. It concludes with information on the qualitative applications of thermoelastic stress analysis.

You do not currently have access to this content.
Don't already have an account? Register

David Backman, 2018. "Thermoelastic Stress Analysis", Nondestructive Evaluation of Materials, Aquil Ahmad, Leonard J. Bond

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal