Skip to Main Content
ASM Handbook

Nondestructive Evaluation of Materials

Edited by
Aquil Ahmad
Aquil Ahmad
Search for other works by this author on:
Leonard J. Bond
Leonard J. Bond
Search for other works by this author on:
ASM International
Volume
17
ISBN electronic:
978-1-62708-190-0
Publication date:
2018
Book Chapter

Guide to Nondestructive Evaluation Techniques

By
Samuel W. Glass, III
Samuel W. Glass, III
Pacific Northwest National Laboratory
Search for other works by this author on:
Published:
2018
Page range:
3 - 7

Abstract

This article provides a discussion on general nondestructive evaluation (NDE) science and considerations for specific technique selection. It explains the basic concept of flaw detection and evaluation and probability of detection. The article provides an overview of NDE methods with their applications, limitations, and advantages. It includes details on NDE codes, calibration standards, inspection frequency, guidance on how to perform inspections, applicability, and mandatory and nonmandatory practice. The article also provides tips on where to focus inspections in order to align with the likely areas of damage or degradation and a number of other aspects of inspection.

You do not currently have access to this content.
Don't already have an account? Register

Samuel W. Glass, III, 2018. "Guide to Nondestructive Evaluation Techniques", Nondestructive Evaluation of Materials, Aquil Ahmad, Leonard J. Bond

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal