Microstructure and Characterization of High-Alloy Cast Irons

By
George F. Vander Voort
George F. Vander Voort
Struers Inc.
Search for other works by this author on:
Juan Asensio-Lozano
Juan Asensio-Lozano
University of Oviedo
(
Asturias
,
Spain
)
Search for other works by this author on:
Published:
2017
Page range:
719 - 732
Publication history
August 28, 2017

Abstract

This article describes two contemporary approaches for preparing cast iron specimens with a wide range of phases and constituents as well as different graphite morphologies. It introduces concepts and preparation materials that enable metallographers to shorten the process while producing better, more consistent results. Recommended procedures to prepare cast irons and examples of high-alloy cast iron microstructures revealed using a variety of etchants are presented. Several etchants are used to reveal the matrix microstructure, depending on the alloy content. The article discusses the use of black and white etchants and lists the compositions of abrasion-resistant cast irons according to ASTM A532/A532M in a table.

You do not currently have access to this content.
Don't already have an account? Register

George F. Vander Voort, Juan Asensio-Lozano, 2017. "Microstructure and Characterization of High-Alloy Cast Irons", Cast Iron Science and Technology, Doru M. Stefanescu

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal