Book Chapter

Castability, Product Design, and Production of Compacted Graphite Irons

By
Steve Dawson
Steve Dawson
SinterCast Limited
Search for other works by this author on:
Wilson Guesser
Wilson Guesser
Tupy S.A. and State University of Santa Catarina
Search for other works by this author on:
Published:
2017
Page range:
665 - 675
Publication history
August 28, 2017

Abstract

The morphology of the graphite particles in compacted graphite iron (CGI) is intermediate to the graphite particles found in gray iron or ductile iron. This article discusses the castability and product design of compacted graphite iron. The introduction of modern measurement and control technologies has made CGI a viable material for high-volume series production. The article describes the production of compacted graphite iron castings and the process control that depends on the production volume of components made from compacted graphite iron. It also discusses the process control for high-volume CGI commonly based on thermal analysis.

You do not currently have access to this content.
Don't already have an account? Register

Steve Dawson, Wilson Guesser, 2017. "Castability, Product Design, and Production of Compacted Graphite Irons", Cast Iron Science and Technology, Doru M. Stefanescu