Book Chapter

Microstructure and Characterization of Compacted Graphite Iron

By
Steve Dawson
Steve Dawson
SinterCast Limited
Search for other works by this author on:
Wilson Guesser
Wilson Guesser
Tupy S.A. and State University of Santa Catarina
Search for other works by this author on:
Published:
2017
Page range:
676 - 685
Publication history
August 28, 2017

Abstract

According to the ISO 16112 standard for compacted graphite cast irons (CGIs), the graphite particles in CGIs shall be predominantly in the vermicular form when viewed on a two dimensional plane of polish. This article begins with a schematic illustration of compacted graphite microstructures with nodularity. It describes the tensile properties, hardness and compressive properties, and impact properties of CGI. The article concludes with a discussion on the fatigue strength and thermal conductivity of CGI.

You do not currently have access to this content.
Don't already have an account? Register

Steve Dawson, Wilson Guesser, 2017. "Microstructure and Characterization of Compacted Graphite Iron", Cast Iron Science and Technology, Doru M. Stefanescu

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal