Skip to Main Content
ASM Handbook

Cast Iron Science and Technology

Edited by
Doru M. Stefanescu
Doru M. Stefanescu
Search for other works by this author on:
ASM International
Volume
1A
ISBN electronic:
978-1-62708-179-5
Publication date:
2017
Book Chapter

Thin-Wall Gray Iron Castings

By
Marcin Górny
Marcin Górny
AGH University of Science and Technology
Search for other works by this author on:
Published:
2017
Page range:
575 - 582
Publication history
August 28, 2017

Abstract

Thin-wall gray cast iron (TWGCI) can be seen as a potential material for the preparation of lightweight castings in automotive engineering applications. This article discusses the most important challenges for TWGCI: cooling rate, solidification, macrostructure, microstructure, and chilling tendency. It reviews the tensile properties and thermophysical properties of gray cast iron. The article describes the variables that influence molten iron preparation: charge materials, melting furnace thermal regime, chemical composition, modification and inoculation treatment, holding time/pouring procedure, mold properties (mold temperature, thermophysical properties of mold and mold coating), and casting design.

You do not currently have access to this content.
Don't already have an account? Register

Marcin Górny, 2017. "Thin-Wall Gray Iron Castings", Cast Iron Science and Technology, Doru M. Stefanescu

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal