Book Chapter

Brazing and Soldering of Cast Irons

By
Charles White
Charles White
Reviewing author
Kettering University
Search for other works by this author on:
Published:
2017
Page range:
310 - 318
Publication history
August 28, 2017

Abstract

Brazing and soldering are done at temperatures below the solidus temperature of the base material but high enough to melt the filler metal and allow the liquid filler metal to wet the surface and spread into the joint gap by capillary action. This article discusses the common advantages of both brazing and soldering. It describes the brazing and soldering of cast irons, as well as the selection of brazing filler material. The article discusses various brazing methods: torch brazing, induction brazing, salt-bath brazing, and furnace brazing. It concludes with information on the application examples of brazing of cast iron.

You do not currently have access to this content.
Don't already have an account? Register

Charles White, 2017. "Brazing and Soldering of Cast Irons", Cast Iron Science and Technology, Doru M. Stefanescu

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal