Skip to Main Content
ASM Handbook

Cast Iron Science and Technology

Edited by
Doru M. Stefanescu
Doru M. Stefanescu
Search for other works by this author on:
ASM International
Volume
1A
ISBN electronic:
978-1-62708-179-5
Publication date:
2017
Book Chapter

Heat Treating of Gray Irons[1]

Published:
2017
Page range:
240 - 255
Publication history
August 28, 2017

Abstract

Gray irons are a group of cast irons that form flake graphite during solidification, in contrast to the spheroidal graphite morphology of ductile irons. This article describes surface hardening of gray irons by flame and induction heating. It provides information on the classification of the gray irons in ASTM specification. The article presents examples that illustrate the use of stress relieving to eliminate distortion and cracking. It describes the three annealing treatments of gray iron: ferritizing annealing, medium (or full) annealing, and graphitizing annealing. The article discusses the parameters of the tensile strength and hardness of a normalized gray iron casting. These include combined carbon content, pearlite spacing, and graphite morphology. The article concludes with a discussion on the induction hardening of gray iron castings.

You do not currently have access to this content.
Don't already have an account? Register

2017. "Heat Treating of Gray Irons", Cast Iron Science and Technology, Doru M. Stefanescu

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal