Skip to Main Content
ASM Handbook

Cast Iron Science and Technology

Edited by
Doru M. Stefanescu
Doru M. Stefanescu
Search for other works by this author on:
ASM International
Volume
1A
ISBN electronic:
978-1-62708-179-5
Publication date:
2017
Book Chapter

Nondestructive Inspection of Cast Irons

By
John A. Griffin
John A. Griffin
The University of Alabama
Search for other works by this author on:
Published:
2017
Page range:
373 - 378
Publication history
August 28, 2017

Abstract

Nondestructive inspection (NDI) methods for cast iron are used to ensure that the parts supplied perform as required by the purchaser. This article focuses on the principal nondestructive methods used to inspect for anomalies in cast irons and to determine if the volume, shape, size, or number of these anomalies exceeds the maximum allowed by the purchaser. The nondestructive methods include visual inspection, dimensional inspection, liquid penetrant inspection, magnetic-particle inspection, eddy-current inspection, radiographic inspection, ultrasonic inspection, resonant testing, and leak testing. The technique, strengths, and weaknesses of each of the nondestructive methods are also discussed.

You do not currently have access to this content.
Don't already have an account? Register

John A. Griffin, 2017. "Nondestructive Inspection of Cast Irons", Cast Iron Science and Technology, Doru M. Stefanescu

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal