Skip to Main Content
ASM Handbook

Cast Iron Science and Technology

Edited by
Doru M. Stefanescu
Doru M. Stefanescu
Search for other works by this author on:
ASM International
Volume
1A
ISBN electronic:
978-1-62708-179-5
Publication date:
2017
Book Chapter

Physical Properties of Cast Irons

By
Doru M. Stefanescu
Doru M. Stefanescu
The Ohio State University and The University of Alabama
Search for other works by this author on:
Published:
2017
Page range:
413 - 429
Publication history
August 28, 2017

Abstract

This article discusses the influence of microstructure and chemical composition on the physical properties of cast iron. The physical properties include density, thermal expansion, thermal conductivity, specific heat, electrical conductivity, magnetic properties, and acoustic properties. The article describes the properties of liquid iron in terms of surface energy, contact angles, and viscosity. The conductive properties such as thermal and electrical conductivity, of the main metallographic phases present in cast iron are presented in a table. The article discusses the magnetic properties of cast iron in terms of magnetic intensity, magnetic induction, magnetic permeability, remanent magnetism, coercive force, and hysteresis loss. It concludes with a discussion on the acoustic properties of cast iron.

You do not currently have access to this content.
Don't already have an account? Register

Doru M. Stefanescu, 2017. "Physical Properties of Cast Irons", Cast Iron Science and Technology, Doru M. Stefanescu

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal