Skip to Main Content
ASM Handbook

Cast Iron Science and Technology

Edited by
Doru M. Stefanescu
Doru M. Stefanescu
Search for other works by this author on:
ASM International
Volume
1A
ISBN electronic:
978-1-62708-179-5
Publication date:
2017
Book Chapter

Volumetric Changes during the Solidification of Cast Iron

By
Attila Diószegi
Attila Diószegi
Jönköping University
,
Sweden
Search for other works by this author on:
Published:
2017
Page range:
88 - 93
Publication history
August 28, 2017

Abstract

Solidification of cast iron alloys brings about volumetric changes. This article describes direct measurements of volume changes with an illustration of the analysis of volumetric changes during solidification of cast iron with the use of a specially designed riser combined with a furnace. It provides a discussion on the dilatometer analysis that is generally used to measure linear displacement as a function of temperature for all types of materials, and the problems associated with volume-change measurements. The article presents a graphical representation of a consequence of the anisotropy, where the calculated volume change is illustrated as a function of temperature. It concludes with a review of kinetic of graphite expansion.

You do not currently have access to this content.
Don't already have an account? Register

Attila Diószegi, 2017. "Volumetric Changes during the Solidification of Cast Iron", Cast Iron Science and Technology, Doru M. Stefanescu

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal