Book Chapter

Heavy-Section Ductile Iron Castings

By
Chantal Labrecque
Chantal Labrecque
Rio Tinto Iron and Titanium
Search for other works by this author on:
Serge Grenier
Serge Grenier
Rio Tinto Iron and Titanium
Search for other works by this author on:
Pierre-Marie Cabanne
Pierre-Marie Cabanne
Rio Tinto Iron and Titanium
Search for other works by this author on:
Martin Gagné
Martin Gagné
Rio Tinto Iron and Titanium
Search for other works by this author on:
Published:
2017
Page range:
629 - 644
Publication history
August 28, 2017

Abstract

This article discusses the production process, testing methods, quality control, and common defects found in heavy-section ductile iron (DI) castings, along with analyses of industrial examples. The common defects include shrinkage defects, graphite-particle-related defects, and chunk graphite defects. The recommended chemical compositions for certain section thicknesses in ductile iron grades are presented in a table. The article illustrates the relationship between microstructure and mechanical properties of DI by using either industrial examples or castings produced under laboratory conditions.

You do not currently have access to this content.
Don't already have an account? Register

Chantal Labrecque, Serge Grenier, Pierre-Marie Cabanne, Martin Gagné, 2017. "Heavy-Section Ductile Iron Castings", Cast Iron Science and Technology, Doru M. Stefanescu

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal