Skip to Main Content
ASM Handbook

Friction, Lubrication, and Wear Technology

Edited by
George E. Totten
George E. Totten
Search for other works by this author on:
ASM International
Volume
18
ISBN electronic:
978-1-62708-192-4
Publication date:
2017
Book Chapter

Solid Particle Erosion[1]

By
Robert J.K. Wood
Robert J.K. Wood
Revising author
University of Southampton
Search for other works by this author on:
Published:
2017
Page range:
266 - 289
Publication history
November 21, 2017

Abstract

Solid particle erosion (SPE) is the loss of material that results from repeated impact of solid particles energized in a carrier fluid. This article reviews important SPE variables, their effects for different classes of materials, composites and coatings, and the mechanisms and theories proposed to explain SPE. It discusses the SPE of metals, steels, and ceramics, as well as erosion of alloys with coarse, nominally two-phase microstructures in which the second-phase particles (SPPs) are typically large compared with the dimensions of the damage zone created by the impact of one particle. The article summarizes the erosion characteristics of polymer matrix composites (PMCs), metal matrix composites (MMCs), ceramic matrix composites (CMCs), and erosion-resistant coatings. The combination of parameters included in most erosion models is also summarized.

You do not currently have access to this content.
Don't already have an account? Register

Robert J.K. Wood, 2017. "Solid Particle Erosion", Friction, Lubrication, and Wear Technology, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal