Friction, Lubrication, and Wear of Internal Combustion Engine Parts

By
Victor W. Wong
Victor W. Wong
Massachusetts Institute of Technology
Search for other works by this author on:
Simon C. Tung
Simon C. Tung
Tung Innovation Technology Consulting Inc.
Search for other works by this author on:
Published:
2017
Page range:
899 - 915
Publication history
November 21, 2017

Abstract

This article focuses on friction, lubrication, and wear of internal combustion engine parts, improvements in which provide important gains in energy efficiency, performance, and longevity of the internal combustion (IC) engine systems. It discusses the types, component materials, and Friction and Wear Control of IC engine. The article explains the process of friction reduction by surface textures or coatings. It provides information on surface hardening of iron and steel, which is commonly employed for engine and powertrain components such as crankshafts, cams, and cylinder liners. The article also discusses advanced surface engineering technologies, such as diamondlike carbon coatings and surface texture technology. Information on thermal-spray methods that have led to improvements in engine components is also provided. The article describes IC engine-components wear, namely, piston assembly wear, valvetrain wear, cylinder-bore wear, and engine bearing wear. It concludes with information on inlet valve and seat wear of IC engine.

You do not currently have access to this content.
Don't already have an account? Register

Victor W. Wong, Simon C. Tung, 2017. "Friction, Lubrication, and Wear of Internal Combustion Engine Parts", Friction, Lubrication, and Wear Technology, George E. Totten