Abstract

This article focuses on environmental and application factors in solid friction. It covers the tribology of contact between a soft and hard material, including mechanisms and testing. The article describes the tribology of contact between a metal and tool during metalworking processes. It also discusses the tribology of metal friction at elevated temperatures.

You do not currently have access to this content.
Don't already have an account? Register

2017. "Environmental and Application Factors in Solid Friction", Friction, Lubrication, and Wear Technology, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal