Coatings and Surface Treatments for Friction and Wear Control

By
Kirsten Bobzin
Kirsten Bobzin
Revising author
RWTH Aachen University—Surface Engineering Institute IOT
Search for other works by this author on:
Mehmet Öte
Mehmet Öte
Revising author
RWTH Aachen University—Surface Engineering Institute IOT
Search for other works by this author on:
Tim Königstein
Tim Königstein
Revising author
RWTH Aachen University—Surface Engineering Institute IOT
Search for other works by this author on:
Lidong Zhao
Lidong Zhao
Revising author
RWTH Aachen University—Surface Engineering Institute IOT
Search for other works by this author on:
Wolfgang Wietheger
Wolfgang Wietheger
Revising author
RWTH Aachen University—Surface Engineering Institute IOT
Search for other works by this author on:
Published:
2017
Page range:
614 - 622
Publication history
November 21, 2017

Abstract

This article describes the technology of thermal spraying with regard to tribological applications. It introduces the basics of tribology and presents the fundamentals of thermal spraying and the relevant process variants and suitable materials. Specific application areas are described regarding the different forms of elementary movement in the corresponding tribological system. The article provides an overview of thermal spray coatings and possible uses for friction and wear control, besides operating as corrosion protection and a thermal barrier. The article provides examples that illustrate how tribological performance can be improved.

You do not currently have access to this content.
Don't already have an account? Register

Kirsten Bobzin, Mehmet Öte, Tim Königstein, Lidong Zhao, Wolfgang Wietheger, 2017. "Coatings and Surface Treatments for Friction and Wear Control", Friction, Lubrication, and Wear Technology, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal