Friction, Lubrication, and Wear of Pump and Compressor Components

By
Toshiharu Kazama
Toshiharu Kazama
Muroran Institute of Technology
Search for other works by this author on:
Published:
2017
Page range:
945 - 956
Publication history
November 21, 2017

Abstract

Pumps and compressors are representative fluid machineries, which are indispensably important industrial equipment for water supply systems, chemical processing and reactions, and fluid power systems. This article addresses friction, lubrication, and wear of components in several types of machines such as positive displacement pumps including hydraulic pumps, turbo-pumps including centrifugal pumps, vacuum pumps, and compressors including the positive displacement type and turbo type.

You do not currently have access to this content.
Don't already have an account? Register

Toshiharu Kazama, 2017. "Friction, Lubrication, and Wear of Pump and Compressor Components", Friction, Lubrication, and Wear Technology, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal