Fretting Wear

By
P.H. Shipway
P.H. Shipway
Revising author
University of Nottingham
Search for other works by this author on:
Published:
2017
Page range:
323 - 336
Publication history
November 21, 2017

Abstract

Fretting is the small-amplitude oscillatory movement that can occur between contacting surfaces, which are nominally at rest. This article discusses fretting wear in mechanical components and the mechanisms of fretting wear. It describes the role of fretting conditions, such as fretting duration, slip amplitude, normal load, fretting frequency, contact geometry, type of vibration, and surface finish, as well as the role of environmental conditions. The article reviews the influence of an aqueous environment on the mechanism of fretting. The steps that can be taken to reduce or eliminate damage due to fretting are extremely diverse. The article presents some general indications of how to address the fretting wear problem.

You do not currently have access to this content.
Don't already have an account? Register

P.H. Shipway, 2017. "Fretting Wear", Friction, Lubrication, and Wear Technology, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal