Tribology and Wear of Bearing Steels[1]

By
C.H. Hager, Jr.
C.H. Hager, Jr.
Revising author
The Timken Company
Search for other works by this author on:
W.M. Hannon
W.M. Hannon
Revising author
The Timken Company
Search for other works by this author on:
V.M. Bedekar
V.M. Bedekar
Revising author
The Timken Company
Search for other works by this author on:
Published:
2017
Page range:
442 - 453
Publication history
November 21, 2017

Abstract

This article discusses the composition, properties and applications of bearing steels. It focuses on the typical wear modes that rolling-element bearings experience: contact fatigue wear, abrasive wear, adhesive wear, and corrosive wear. The article provides information on reliability factor and ABMA and ISO environmental factors.

You do not currently have access to this content.
Don't already have an account? Register

C.H. Hager, Jr., W.M. Hannon, V.M. Bedekar, 2017. "Tribology and Wear of Bearing Steels", Friction, Lubrication, and Wear Technology, George E. Totten