Skip to Main Content
ASM Handbook

Friction, Lubrication, and Wear Technology

Edited by
George E. Totten
George E. Totten
Search for other works by this author on:
ASM International
Volume
18
ISBN electronic:
978-1-62708-192-4
Publication date:
2017
Book Chapter

Carburizing

By
Allen J. Fuller, Jr.
Allen J. Fuller, Jr.
Amsted Rail Company, Inc.
Search for other works by this author on:
Published:
2017
Page range:
634 - 637
Publication history
November 21, 2017

Abstract

This article reviews the factors influencing carburization to improve wear resistance of steel, such as operating temperature, cost, production volume, types of wear, and design criteria. It details the types of wear, namely abrasive wear and adhesive wear. The article discusses the characteristics of carburized steels that affect wear resistance, including hardness, microstructure, retained austenite, and carbides. It also describes the processing considerations for carburization of titanium.

You do not currently have access to this content.
Don't already have an account? Register

Allen J. Fuller, Jr., 2017. "Carburizing", Friction, Lubrication, and Wear Technology, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal