Wear Particle Analysis

By
Noam Eliaz
Noam Eliaz
Tel-Aviv University
Search for other works by this author on:
Published:
2017
Page range:
1010 - 1031
Publication history
November 21, 2017

Abstract

This article focuses on different aspects of wear particle analysis. It discusses the different wear regimes in the wear rate versus time (bathtub) curve. The article explains the essence of condition monitoring and how to properly sample lubricants for condition monitoring. It also discusses in-service lubricant analysis for condition monitoring, focusing on the spectrometric oil analysis program. The article describes the characteristics of wear particles and analytical techniques for characterizing them. It also describes the characteristics of different types of wear particles and the mechanisms by which they are generated. The article concludes with a summary of the major applications of wear particle analysis.

You do not currently have access to this content.
Don't already have an account? Register

Noam Eliaz, 2017. "Wear Particle Analysis", Friction, Lubrication, and Wear Technology, George E. Totten