Friction and Wear of Sliding Bearings

By
Harish Hirani
Harish Hirani
IIT Delhi and Central Mechanical Engineering Research Institute
,
India
Search for other works by this author on:
Published:
2017
Page range:
819 - 835
Publication history
November 21, 2017

Abstract

Bearings are usually provided where a specific spatial relationship (alignment) must be maintained between the parts or where a force is to be transmitted from one part to the other. This article introduces the general types and configuration of sliding bearings, bearing materials, and the practical aspects and solutions in the friction, lubrication, and wear mitigation of sliding bearings. The lubrication of bearings includes thick-film lubrication, thin-film lubrication, and boundary lubrication. The article concludes with a discussion on the effects of material elasticity on the lubrication of bearings.

You do not currently have access to this content.
Don't already have an account? Register

Harish Hirani, 2017. "Friction and Wear of Sliding Bearings", Friction, Lubrication, and Wear Technology, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal