Introduction to Condition Monitoring

By
Zakwan Skaf
Zakwan Skaf
Cranfield University
Search for other works by this author on:
Published:
2017
Page range:
1005 - 1009
Publication history
November 21, 2017

Abstract

This article introduces the concept of condition monitoring (CM) and summarizes various techniques used for CM across the industrial sectors. The techniques include visual inspection, performance monitoring, vibration condition monitoring, vibration condition monitoring, lubricant oil analysis, acoustic emission testing, temperature monitoring, motor current signature analysis, and ultrasound emission. The article describes the evolution of condition-based maintenance in CM. It also describes the basics of integrated vehicle health management, a capability that enables a number of maintenance philosophies. The article concludes with a discussion on various condition monitoring in industrial sectors, including condition-monitoring techniques in nuclear power plants, road condition monitoring, and condition monitoring in wind turbines.

You do not currently have access to this content.
Don't already have an account? Register

Zakwan Skaf, 2017. "Introduction to Condition Monitoring", Friction, Lubrication, and Wear Technology, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal