Book Chapter

Ionic Liquids as Lubricants or Lubricant Additives

By
Huaping Xiao
Huaping Xiao
China University of Petroleum
Search for other works by this author on:
Shuhai Liu
Shuhai Liu
China University of Petroleum
Search for other works by this author on:
Published:
2017
Page range:
169 - 183
Publication history
November 21, 2017

Abstract

This article introduces the structure, tribological properties, advantages, and applications of ionic liquids (ILs) as lubricating media. It discusses the mechanisms of IL lubrication for different contacts. The advances in studies focusing on tribological properties of a wide range of ILs are reviewed. The article concludes with the challenges that limit the applications of ILs in tribology engineering.

You do not currently have access to this content.
Don't already have an account? Register

Huaping Xiao, Shuhai Liu, 2017. "Ionic Liquids as Lubricants or Lubricant Additives", Friction, Lubrication, and Wear Technology, George E. Totten