Skip to Main Content
ASM Handbook

Friction, Lubrication, and Wear Technology

Edited by
George E. Totten
George E. Totten
Search for other works by this author on:
ASM International
Volume
18
ISBN electronic:
978-1-62708-192-4
Publication date:
2017
Book Chapter

Carbide- and Boride-Based Thick Coatings for Abrasive Wear-Protection Applications

By
W. Theisen
W. Theisen
Ruhr-Universitat Bochum
Search for other works by this author on:
A. Röttger
A. Röttger
Ruhr-Universitat Bochum
Search for other works by this author on:
Published:
2017
Page range:
597 - 613
Publication history
November 21, 2017

Abstract

This article provides a brief introduction to abrasive wear-resistant coating materials that contain a large amount of hard phases, such as borides, carbides, or carboborides. It describes some of the commonly used methods of producing thick wear-resistant coatings. The article also provides information on metal-matrix composites and cemented carbides. The three base-alloying concepts, including cobalt-, iron-, and nickel-base alloys used for wear-protection applications, are also described. The article compares the tribomechanical properties of the materials in a qualitative manner, thus allowing a rough materials selection for practitioners. It presents a brief discussion on hot isostatic pressing (HIP) cladding, sinter cladding, and manufacturing of thick wear-resistant coatings by extrusion or ring rolling. The article also discusses the processing sequence of thick wear-resistant coatings, namely, compound casting, deposition welding, and thermal spraying.

You do not currently have access to this content.
Don't already have an account? Register

W. Theisen, A. Röttger, 2017. "Carbide- and Boride-Based Thick Coatings for Abrasive Wear-Protection Applications", Friction, Lubrication, and Wear Technology, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal