Skip to Main Content
ASM Handbook

Friction, Lubrication, and Wear Technology

Edited by
George E. Totten
George E. Totten
Search for other works by this author on:
ASM International
Volume
18
ISBN electronic:
978-1-62708-192-4
Publication date:
2017
Book Chapter

Friction and Wear of Seals

By
George K. Nikas
George K. Nikas
KADMOS Engineering Ltd.
Search for other works by this author on:
Published:
2017
Page range:
957 - 968
Publication history
November 21, 2017

Abstract

Seals are mechanical components that prevent the leakage, diffusion, transfer, or mixing of different liquid, gas, solid, and multiphasic substances. This article begins by discussing the classifications of seals: static and dynamic. Static seals involve both self-energizing elastomeric materials such as O-rings, which merely react to a sealed fluid pressure, and passive materials that require clamping forces to achieve sealing, such as gaskets. The types of dynamic seals include rotary seals and reciprocating seals. The article describes the factors affecting seal wear and failure. It provides a list of some common seal wear modes and failures, namely abrasion, cavitation damage, chemical attack, compression set, corrosion, damage during abrupt decompression, dieseling damage, extrusion damage, installation damage, spiral or rolling damage, and vaporization damage. The article concludes with specific recommendations for reducting of seal friction and wear.

You do not currently have access to this content.
Don't already have an account? Register

George K. Nikas, 2017. "Friction and Wear of Seals", Friction, Lubrication, and Wear Technology, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal