Skip to Main Content
ASM Handbook

Friction, Lubrication, and Wear Technology

Edited by
George E. Totten
George E. Totten
Search for other works by this author on:
ASM International
Volume
18
ISBN electronic:
978-1-62708-192-4
Publication date:
2017
Book Chapter

Carbon-Base (Diamondlike and Diamond) Coatings

By
Ryan D. Evans
Ryan D. Evans
The Timken Company
Search for other works by this author on:
Published:
2017
Page range:
571 - 582
Publication history
November 21, 2017

Abstract

This article describes two variations of carbon-base coatings: diamondlike carbon (DLC) coatings and polycrystalline diamond (PCD) coatings. It discusses the basics of a few deposition methods as they apply to industrially relevant coatings. The methods include deposition of tungsten-containing hydrogenated amorphous carbon films, deposition of tetrahedral amorphous carbon films, and deposition of silicon-incorporated hydrogenated amorphous carbon films. The most common deposition technologies for diamond films are also discussed. The article provides information on surface preparation for DLC and diamond deposition. It also provides a discussion on the coating composition and structure, mechanical and tribological properties, and applications of DLC and diamond coatings. The quality control techniques for DLC and diamond coatings are specified to meet customer requirements and ensure repeatable quality.

You do not currently have access to this content.
Don't already have an account? Register

Ryan D. Evans, 2017. "Carbon-Base (Diamondlike and Diamond) Coatings", Friction, Lubrication, and Wear Technology, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal