Skip to Main Content
ASM Handbook

Friction, Lubrication, and Wear Technology

Edited by
George E. Totten
George E. Totten
Search for other works by this author on:
ASM International
Volume
18
ISBN electronic:
978-1-62708-192-4
Publication date:
2017
Book Chapter

Polyalphaolefin Lubricant Applications

By
Ken Hope
Ken Hope
Chevron Phillips Chemical Company LP
Search for other works by this author on:
Published:
2017
Page range:
207 - 212
Publication history
November 21, 2017

Abstract

This article presents a brief discussion on the main applications for low- and high-viscosity polyalphaolefins (PAOs) and highlights key areas of interest and shows why PAOs are used in these applications. It discusses the physical properties of passenger car motor oils (PCMOs) based on or containing PAOs. The properties include Noack volatility and pour point. The article also discusses the properties and applications of heavy-duty engine oil (HDEO), industrial lubricants, food-grade lubricants, greases, transportation gear oils, compressor oils, hydraulic fluids, and transmission fluids.

You do not currently have access to this content.
Don't already have an account? Register

Ken Hope, 2017. "Polyalphaolefin Lubricant Applications", Friction, Lubrication, and Wear Technology, George E. Totten