Chemically Assisted and Environmentally Controlled Wear

Published:
2017

Abstract

Tribocorrosion is the subject dealing with complex, synergistic effects of chemical and mechanical conditions that cause wear. This article begins with a discussion on oxidative wear and corrosive wear, as well as quantitative measurements of corrosion, mechanical wear, and wear-corrosion effects. It illustrates the mechanism of corrosive-abrasive wear and discusses the factors affecting two-body wear. These factors include particle shape, size, density, and hardness; slurry velocity; slurry particle angle of attack; solids concentration in the slurry; hydrodynamic factors; corrosion products and the mass transfer of oxygen. The article describes slurry particle impingement tests and grinding tribocorrosion tests, as well as the factors to be considered for mitigating corrosive wear, such as materials selection, surface treatments, and environment modifications.

You do not currently have access to this content.
Don't already have an account? Register

2017. "Chemically Assisted and Environmentally Controlled Wear", Friction, Lubrication, and Wear Technology, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal