Mechanical Properties of Carbon and Alloy Steels

Published:
1998
Page range:
219 - 225

Abstract

The properties of carbon and alloy steels are dependent on the relationships between chemical composition, processing, and microstructure. This article discusses the effects of alloying and residual elements on the mechanical properties of carbon and alloy steels. Tables listing values for the mechanical properties of selected carbon and alloy steels in the hot-rolled, normalized, annealed, and quenched-and tempered condition are provided.

You do not currently have access to this content.
Don't already have an account? Register

1998. "Mechanical Properties of Carbon and Alloy Steels", Metals Handbook Desk Edition, Joseph R. Davis

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal