Crystal Structure of Metallic Elements

By
Hugh Baker
Hugh Baker
ASM International
Search for other works by this author on:
Published:
1998
Page range:
88 - 95

Abstract

Crystal structure is the arrangement of atoms or molecules in the solid state that involves consideration of defects, or abnormalities, in idealized atomic/molecular arrangements. The three-dimensional aggregation of unit cells in the crystal forms a space lattice or Bravais lattice. Providing a brief review of the terms and basic concepts associated with crystal structures, this article discusses some of the significant defects obstructing plastic flow in real crystals, namely point defects, line defects, stacking faults, twins, and cold work. Several tables provide information on the crystal structures and lattice parameters of allotropes of metallic elements.

You do not currently have access to this content.
Don't already have an account? Register

Hugh Baker, 1998. "Crystal Structure of Metallic Elements", Metals Handbook Desk Edition, Joseph R. Davis