Classifications and Designations of Carbon and Alloy Steels

Published:
1998
Page range:
203 - 219

Abstract

This article provides an overview of the different classification and designation systems of wrought carbon steel and alloy steel product forms with total alloying element contents not exceeding 5″. It lists the quality descriptors, chemical compositions, cast or heat composition ranges, and product analysis tolerances of carbon and alloy steels. The major designation systems discussed include the Society of Automotive Engineers (SAE)-American Iron and Steel Institute (AISI) designations, Unified Numbering System (UNS) designations, American Society for Testing and Materials (ASTM) designations, Aerospace Material Specification (AMS), and other international designations and specifications.

You do not currently have access to this content.
Don't already have an account? Register

1998. "Classifications and Designations of Carbon and Alloy Steels", Metals Handbook Desk Edition, Joseph R. Davis

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal