Basic Metallurgy of Cast Iron

Published:
1998
Page range:
307 - 309

Abstract

Cast irons are primarily iron alloys that contain more than 2% carbon and from 1 to 3% silicon. This Article provides a description of the iron-iron carbide-silicon system and discusses the classification, composition, and characteristics of cast irons, such as gray, ductile, malleable, compacted graphite, and white cast iron. A table shows the correspondence between the commercial and microstructural classifications as well as the final processing stage in obtaining common cast irons.

You do not currently have access to this content.
Don't already have an account? Register

1998. "Basic Metallurgy of Cast Iron", Metals Handbook Desk Edition, Joseph R. Davis